溫州興發(fā)保潔服務(wù)告訴您地坪表面有刷痕
環(huán)氧地坪表面刷痕產(chǎn)生的原因:
A、施工原因:施工方法錯誤,涂料攪拌后施工時間過長,滾刷均勻,涂層薄厚控制不到位。
B、工具原因:滾筒質(zhì)量不合格,滾筒表面處理有誤。
C、涂料本身的原因:主要是涂料的流平性差,涂料的粘度過高。有觸變性的填料或助劑。
解決的方法:
A、注意施工方法,涂料的成都保潔公司熟化時間不要過長。滾筒的二端到圓角,涂層的一遍厚度盡可能不要小于0.15mm。
B、買好一點的滾筒,滾筒使用前用膠帶處理一下滾筒表面
C、涂料的原因,增加涂料的流平性,降低涂料的粘度,盡可能減少有觸變性的填料和助劑,特別要注意墻面涂料的流平劑用在地坪涂料的現(xiàn)象。
The causes of floor surface brush marks:
A, the construction: construction method error, coating construction time is too long, after mixing uniform roller, coating and its thickness control does not reach the designated position.
B, tool reason: quality unqualified roller, roller surface treatment is wrong.
C, the cause of the coating itself: mainly poor flowing property of paint, paint viscosity is too high. Has thixotropy fillers or additives.
The solution:
A, pay attention to the construction methods, coating curing time not too long. The two end of the cylinder to the rounded corners, coating thickness again as far as possible do not less than 0.15 mm.
B, bought a bit of roller, roller tape with the roller surface before using
C, coating, increase the coating flow property, lower the viscosity of the coating, minimize has thixotropy fillers and additives, special attention should be paid to metope paint flow ping agent on the phenomenon of floor coating.